Product Details:
|
| Nd:YVO4 Doping: | 0.1-3% | Nd:YAG Doping: | 0.1-3% |
|---|---|---|---|
| Wavefront Distortion: | < λ /8 At 633 Nm | Orientation: | ±0.5deg |
| Scratch/Dig: | 10/5@MIL-O-13830A | Flatness: | λ /10 At 633 Nm |
| Clear Aperture: | > Central 90% | Parallelism: | < 10 Arc Seconds |
| Intrinsic Loss: | < 0.1% Cm -1 | Coating:: | AR Or HR Coating |
| Highlight: | compact diffusion bonding crystals,High damage threshold bonding crystals,Decrease thermal effect Laser Crystals |
||
Technical Specifications:
| Material | Doping Concentration | Aperture (mm) | Length (mm) |
| Nd:YAG+Cr4+:YAG | 0.1-3%/0.6-7.0 | 2×2-20×20 | 0.5-200 |
| YAG+Nd:YAG | 0.1-3% | 2×2-20×20 | 0.5-200 |
| YAG+Nd:YAG+YAG | 0.1-3% | 2×2-20×20 | 0.5-200 |
| YAG+Nd:YAG+Cr4+:YAG | 0.1-3%/0.6-7.0 | 2×2-20×20 | 0.5-200 |
| YVO4+Nd:YVO4 | 0.1-3% | 2×2-20×20 | 0.5-200 |
| YVO4+Nd:YVO4+YVO4 | 0.1-3% | 2×2-20×20 | 0.5-200 |
| YVO4+Nd:YVO4+YVO4 | 0.1-3% | Dia2-15 | 0.5-200 |
| Nd:YVO4 Doping | 0.1-3% |
| Nd:YAG Doping | 0.1-3% |
| Wavefront Distortion | < λ /8 at 633 nm |
| Orientation | ±0.5deg |
| Scratch/Dig | 10/5@MIL-O-13830A |
| Flatness | λ /10 at 633 nm |
| Clear Aperture | > Central 90% |
| Parallelism | < 10 arc seconds |
| Intrinsic Loss | < 0.1% cm -1 |
| Coating: | AR or HR coating |
Contact Person: Mr. JACK HAN
Tel: 86-18655618388